Fastening System Performance in Very High-Temperature Regions

Nov 28, 2025 Leave a message

Thermal Loads the System Has to Carry

Rail steel expands and contracts with temperature at about 11.5 millionths per degree Celsius. On a desert route the rail can reach well above 60 C in the afternoon sun and fall close to freezing at night, so the stress-free temperature chosen at installation determines the compressive force in the rail at the hottest part of the day and the tensile force in the coldest. The fastener does not remove that force, but it must keep the rail foot seated, hold gauge and prevent rail rollover while the rail moves within the fastening assembly.

Metal components expand too. Screw spikes and bolts, shoulders and baseplates all grow with temperature, and differential expansion between a steel fastener and a concrete or composite sleeper changes the preload in the assembly. Design calculations therefore use the actual service temperature band, not the ambient air temperature.

Material Selection for Sustained Heat

Component Typical choice Why it matters in heat Test reference
Elastic clip 60Si2MnA spring steel to GB/T 1222 Retains clamping force, limited stress relaxation ASTM E328, ISO 6508-1
Rail pad EPDM or thermoplastic polyester elastomer Low creep and low set at high pad temperature EN 13146 series
Insulator Glass-filled polyamide or ceramic Shape retention and electrical resistance EN 13146 series
Coating Zinc flake or hot dip galvanizing Barrier against dust-borne and chemical corrosion ISO 10683, EN ISO 1461, ISO 9227

Stress relaxation is the quiet failure mode. A clip that loses a fraction of its clamping force after a summer of sustained heat may still pass a visual check, which is why relaxation testing to ASTM E328 is specified where service temperature is high.

Functional Requirements to Write into the Specification

A specification for a hot-region fastening system should require: clamping force at installed deflection with an upper and lower limit; retention of that force after thermal cycling; torsional resistance so that the rail cannot roll under lateral load; longitudinal restraint consistent with the continuous welded rail design; and electrical resistance suitable for the signalling system. The EN 13481 series sets these requirements by application, and the EN 13146 series provides the test methods for longitudinal restraint, torsional resistance, repeated loading, electrical resistance and severe environmental exposure.

Dust, Sand and Chemical Exposure

Abrasive dust works on sliding surfaces: the contact between clip toe and insulator, and between insulator and rail foot. Where dust ingress is heavy, pad and insulator geometry should include a sealing lip. In industrial zones the additional load is chemical, with acidic and alkaline deposits attacking coatings and, in the worst case, stress corrosion at threaded parts. Coating systems are selected and verified by neutral salt spray to ISO 9227, with galvanizing assessed to EN ISO 1461 and zinc flake coatings to ISO 10683. Polymeric components are checked for ultraviolet degradation by exposure testing, for example to ISO 4892-2 or ASTM G154.

Verification, Installation and Maintenance

Verification should combine component testing with assembly testing. Repeated loading of the assembled fastening, in line with the EN 13146 series and evaluated against the EN 13481 acceptance requirements, is the test that best represents service. On site, hold the installation torque or driving depth within the stated range, because over-driving raises preload in heat and under-driving loses clamping force. Gauge and cross level are then monitored under EN 13848-1. Track circuits need the insulation resistance of the assembly to stay above the signalling threshold, which is why the electrical resistance test belongs in the type approval file.

Frequently Asked Questions

Q: How hot does rail actually get in a desert?
A: Rail temperature in full sun is typically 20-30 C above local air temperature, so a 45 C afternoon can put the rail above 65 C. Design work should use a measured rail temperature band, not air temperature alone.

Q: Why does stress relaxation matter more than hardness?
A: Hardness tells you about wear resistance at the seat; relaxation tells you whether the clip still holds the rail foot after months at high temperature. A clip can keep its hardness and still lose clamping force through relaxation.

Q: Which standard governs fastening system acceptance?
A: The EN 13481 series sets the performance requirements by track application, and the EN 13146 series gives the test methods used to demonstrate longitudinal restraint, torsional resistance, repeated loading, electrical resistance and environmental exposure.

Q: Is galvanizing enough for a coastal industrial zone?
A: Not always. Hot dip galvanizing to EN ISO 1461 performs well in many environments, but in aggressive chemical or chloride exposure a zinc flake system to ISO 10683 or a duplex coating is often specified, with salt spray evidence to ISO 9227.

Q: How is a hot-region fastening system qualified?
A: By component tests for chemistry and hardness, relaxation testing where high temperature applies, and full assembly testing for clamping force, repeated loading and electrical resistance, supported by inspection documents to EN 10204 grade 3.1.