Thread Rolling Forming Process and Pull-out Resistance Enhancement Design for Rail Spikes

Jan 29, 2026 Leave a message

Thread Rolling Forming Process and Pull-out Resistance Enhancement Design for Rail Spikes

 

What are the process performance differences between thread rolling forming and traditional cutting forming of rail spikes?

The core performance differences between thread rolling forming and traditional cutting forming of rail spikes are reflected in three aspects: substrate integrity, stress distribution and mechanical strength. Thread rolling forming forms threads through cold plastic deformation without material cutting, the metal fibers of the spike shank are continuous and intact, and no microcracks caused by cutting are generated, while cutting forming cuts off metal fibers and forms a stress concentration area at the root of the thread. The thread root after rolling forming is an arc transition, the stress peak is reduced by more than 40% compared with cutting forming, which can effectively resist the repeated tensile stress caused by train vibration, and the thread root of cutting forming is a right angle, which is easy to initiate fatigue cracks. In terms of mechanical strength, rolling forming increases the hardness of the spike thread area to HRC38-42, the tensile strength is ≥600MPa, and the pull-out resistance is 35% higher than that of cutting formed spikes. The hardness of the cutting formed spike thread area is only HRC28-32, and the tensile strength is less than 450MPa. In addition, the production efficiency of rolling forming is 2-3 times that of cutting forming, the material utilization rate can reach 100%, which greatly reduces the production cost, while the material loss rate of cutting forming is about 15%-20%. The thread surface of the roll-formed spike is smoother with a roughness Ra≤1.6μm, which reduces the meshing wear with the sleeper nut, and the surface roughness of the cut-formed thread is Ra≥3.2μm, which is prone to thread slipping during meshing.

 

rail spike fatcory

 

What is the action principle of the inverted conical shank design of rail spikes to enhance pull-out resistance?

The core principle of the inverted conical shank design of rail spikes to enhance pull-out resistance is that the taper structure of the shank makes the contact area between the spike and the sleeper increase gradually when the spike is under tension, forming a "wedge effect", and at the same time disperses the tensile stress to avoid local stress concentration. The taper of the inverted conical shank is controlled at 1:50-1:40, and the diameter decreases gradually from the nail head to the nail tip. When the spike is subjected to the pulling force generated by train vibration, the conical side of the shank will be closely attached to the wall of the reserved hole of the sleeper, the contact area increases with the increase of the pulling force, and the positive pressure of the hole wall on the spike also increases synchronously, thereby increasing the friction between the two and offsetting part of the pulling force. Compared with the traditional cylindrical shank, the contact between the inverted conical shank and the sleeper is surface contact rather than line contact, the tensile stress is evenly distributed on the entire conical contact surface, and no stress peak is formed at a certain part, which effectively prevents the cracking of the reserved hole wall of the sleeper. In addition, the root of the inverted conical shank and the nail head adopt an arc transition with a curvature radius of 8-10mm, which further eliminates stress concentration and improves the stability of the connection between the spike and the sleeper. In actual service, the pull-out loosening rate of inverted conical spikes is 60% lower than that of cylindrical spikes, which can maintain a firm connection with sleepers for a long time and avoid rail displacement caused by spike loosening.

 

rail-road-spike

 

What are the adaptive design requirements of rail spikes for different sleeper types?

The adaptive design of rail spikes for different sleeper types is to adjust the shank taper, thread specification and nail tip structure to match the material characteristics and fixing requirements of concrete sleepers, wooden sleepers and steel sleepers. Concrete sleepers have high hardness and strong integrity, the adapted spikes adopt 1:45 inverted conical shank, M24×1.5 fine thread with a thread length of 80mm, the nail tip is triangular, which is easy to drive into the reserved hole and form mechanical interlock with concrete, the pull-out resistance needs to be ≥80kN to meet the fixing requirements of heavy-haul lines. Wooden sleepers are soft and easy to deform, the adapted spikes adopt 1:50 small taper shank, M20×2 coarse thread with a thread length of 60mm to increase the meshing area with wood, the nail tip is beveled to reduce the splitting damage to wooden sleepers during driving, and the nail shank is equipped with annular anti-slip lines to improve the friction with wooden sleepers and prevent spike rotation and loosening. Steel sleepers have high strength and rigidity, the adapted spikes adopt equal-section threaded shank (no taper), M22×1.5 fine thread, the nail head is hexagonal flange type, which increases the contact area with steel sleepers, the bolt tightening torque is controlled at 300-350N·m, and the fixing is realized by the pressing force of the flange surface. The spikes need to be overall hot-dip galvanized to improve the anti-corrosion adaptability with steel sleepers.

 

Gnee rail spikes

 

What are the surface anti-corrosion treatment processes of rail spikes and their adaptive environmental requirements?

The surface anti-corrosion treatment processes of rail spikes mainly include hot-dip galvanizing, dacromet coating and zinc infiltration treatment. Different processes have different anti-corrosion performances and need to be adapted according to the corrosion intensity of the service environment. Hot-dip galvanizing is a basic anti-corrosion method with a galvanized layer thickness of 80-100μm, which protects the spike substrate through the sacrificial anode effect of the zinc layer, adapted to the inland dry line environment with low corrosion degree. This process has low cost and simple construction, which can meet the anti-corrosion requirements of general lines. Dacromet coating is a mid-to-high end anti-corrosion method with a coating thickness of 60-80μm, composed of zinc powder, aluminum powder and binder, with excellent salt spray and damp heat resistance, the neutral salt spray test can reach 1000 hours without red rust, adapted to coastal high salt spray, rainy and humid line environments, and the coating has no hydrogen embrittlement risk, suitable for the anti-corrosion treatment of high-strength spikes. Zinc infiltration treatment is a high-end anti-corrosion method, zinc atoms penetrate into the spike substrate to form an alloy layer with a thickness of 50-70μm and a bonding strength of ≥100MPa, with excellent wear and corrosion resistance, the salt spray test can reach more than 1500 hours, adapted to the dark and humid, dusty tunnel environment and alpine line environment with frequent use of snow melting agents. The zinc infiltration layer is metallurgically bonded with the spike substrate, and no coating falling off will occur. In addition, in a particularly severe corrosion environment, "hot-dip galvanizing + closed coating" composite anti-corrosion can be adopted to further improve the anti-corrosion life of the spike.

 

What are the core points of on-site installation and anti-loosening maintenance of rail spikes?

The core points of on-site installation and anti-loosening maintenance of rail spikes are to ensure installation verticality, control tightening torque, and conduct regular anti-loosening re-inspection to ensure a firm connection between the spike and the sleeper. Before installation, clean the debris and scum in the reserved hole of the sleeper, check the surface state of the spike, only spikes without rust and thread damage can be used. The reserved hole of concrete sleeper needs to be filled with anchoring agent in advance, and the strength grade of the anchoring agent should be ≥C40 to ensure the bonding strength with the spike. During installation, the spike must be kept perpendicular to the top surface of the sleeper with a verticality deviation ≤1°, to avoid uneven contact between the spike and the hole wall caused by skew of the spike and form local stress concentration. The wooden sleeper spike is driven in with a special nail driver, and it is strictly forbidden to strike directly with a hammer to prevent bending of the nail shank or splitting of the wooden sleeper. When tightening the nut, use a torque wrench to control the torque according to the sleeper type: the torque of concrete sleeper spike is 250-300N·m, and that of steel sleeper spike is 300-350N·m. Over-torque tightening is strictly forbidden to prevent thread slipping of the spike or fracture of the shank. The inspection cycle of daily maintenance is 3 months, focusing on checking whether the spike is loose and whether the nut is falling off, recheck the tightening torque with a torque wrench, and retighten in time if the torque attenuation exceeds 10%. For small-radius curve sections with frequent vibration, the spike should be equipped with anti-loosening washers or double nuts to prevent loosening caused by high-frequency vibration. If the spike is severely rusted or the thread slips, it must be replaced immediately. When replacing, clean the old anchoring agent and refill with new anchoring agent to ensure the fixing strength of the new spike.